Bathtub entrance decoration cement Barbed Wire,Electro Galvanized Barbed Wire,Galvanized Barbed Wire Xinlong Wire Mesh Manufacture Co., Ltd. , http://www.hebwiremesh.com
1. Checkpoints at the grassroots level: ground cleaning is in place;
The grass-roots surface is flat and there must be no hesitation, hollowing, delamination, cracking;
Pipes, corner roots, floor drains, and yin and yang corners on the walls require 1:1 cement mortar as an additional waterproof layer;
Wall and ground yin and yang angles should be rounded;
2, coating waterproof, water closed test checkpoint: waterproof layer should extend from the ground to the wall, higher than the ground 0.3m; such as the installation of the bathtub, the waterproof layer is 20cm higher than the edge of the bathtub.
The paint brush shall be uniform and shall not leak the brush;
The coating brushing should be carried out in batches, and the coating can be continued until the upper layer is dry.
Coating film protection work during coating interval;
The closed water test time is 24 hours (water depth is 2 cm) and must not be advanced;
When checking, focus on the root of the pipeline, the angle between the yin and yang, and the location of the water-resistant transformation of the hydropower station
Found that the leakage of water phenomenon should be proposed and dealt with in a timely manner;
Xi'an renovation classroom walls, ground waterproofing